BCUP-3
Ramp rate should be as quick as possible while brazing;Joints become bright gray, returning to original copper color once dipped into a 10% sulfuric solution.
Products Description
Comments
Brazing Alloy | Composition(%) | Melting Range(℃) | Applicable scope | ||||
Ag | Cu | P | Sn | Solidus | Liquidus | ||
HL205 (as:BCUP-3) |
5±0.5 | Balance | 6.0 | 640 | 800 | Ramp rate should be as quick as possible while brazing;Joints become bright gray, returning to original copper color once dipped into a 10% sulfuric solution. |